This paper reports on an experimental investigation into the axial and lateral strain development of fiber reinforced polymer (FRP) confined high-strength concrete (HSC) with prestressed FRP shells. A total of 24 aramid FRP (AFRP)-confined concrete specimens were manufactured as concrete-filled FRP tubes (CFFTs) with instrumentation to measure the strain variations during application of prestress, removal of end constraints and progressive prestress losses. Prestressed CFFT specimens were prepared with three different dose rates of expansive mineral admixture to create a range of lateral prestress applied to AFRP tubes manufactured with sheet thicknesses of 0.2 or 0.3 mm/ply and referred to as lightly- or well-confined, respectively. In addition to these three levels of prestress, non-prestressed companion specimens were manufactured and tested to determine baseline performance. The experimental results from this study indicate that lateral prestressing of CFFTs manufactured with HSC can be achieved by varying the expansive mineral admixture dose rate with a lateral prestress of up to 7.3 MPa recorded in this study. Significant strain variations were measured during removal of the end constraints with up to 700 microstrain recorded in the axial direction. Finally, the measurement of prestress losses for the month following prestress application revealed minimal progressive losses, with only 250 and 100 με recorded for the axial and hoop strains, respectively.
机译:这在试验调查纤维的轴向和横向应变发展文件报告增强的聚合物(FRP)局限于高强度混凝土(HSC)预应力FRP壳。共有24个芳族聚酰胺FRP(AFRP)-confined混凝土试样制造混凝土填充FRP管(CFFTs)与仪表应用预应力,拆除端约束和渐进的损失预应力期间测量的应变的变化。预应力CFFT标本进行膨胀矿物外加剂的三种不同的剂量率制备的施加到具有0.2或0.3毫米/帘布层的板厚制造AFRP管横向预应力和分别被称为lightly-或-局限于井,以创建一个范围。除了这三个层次的预应力,非预应力伴侣样品制造和测试,以确定基线表现。从这项研究中的实验结果表明,与HSC制造CFFTs的横向预应力可以通过与至7.3兆帕记录在该研究最多的横向预应力改变膨胀矿物外加剂剂量率来实现。与记录在轴向方向上高达700微应变去除的末端约束期间测量显著应变变化。最后,用于以下应用预应力月预应力损失测定结果表明最小的渐进损失,只有250和100分别με记录的轴向和环向应变。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号