Magnetic properties of powder hard magnetic Fe-27Cr-10Co-0.5Mo and Fe-27Cr-10Co-2Mo alloys

机译:粉末硬磁Fe-27Cr-10Co-0.5Mo和Fe-27Cr-10Co-2Mo合金的磁性

获取原文

摘要

Magnetic hysteresis properties of powder hard magnetic Fe-27Cr-10Co alloys with 0.5 and 2.0 wt % molybdenum were studied. For Fe-27Cr-10Co-0.5Mo alloy: Br = 1.35 T,H_(cB) = 45.6 kA/m and (BH)_(max) = 41 kJ/m~3. For Fe-27Cr-10Co-2Mo alloy: Bt = 1.29 T, H_(cB) = 41 kA/m, (BH)_(max) = 34.8 kJ/m~3. It was shown that an alloying with 2 wt. % molybdenum of the low-cobalt powder hard magnetic Fe-27Cr-lOCo alloy unlike high-cobalt hard magnetic FeCrCo alloys did not increase its magnetic hysteresis properties, reduced the camber of a demagnetization curve in a second quadrant.
机译:研究了粉末硬磁Fe-27CR-10CO合金的磁滞性能,具有0.5和2.0wt%钼。对于FE-27CR-10CO-0.5MO合金:BR = 1.35 T,H_(CB)= 45.6 ka / m和(BH)_(max)= 41 kJ / m〜3。对于FE-27CR-10CO-2MO合金:BT = 1.29 T,H_(CB)= 41 kA / m,(BH)_(MAX)= 34.8 kJ / m〜3。结果表明,合金化用2重量%。低钴粉硬磁FE-27CR-LOCO合金的%钼与高钴硬磁性FECRCO合金不同,不增加其磁滞的特性,在第二象限中减少了退磁曲线的弯曲。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号