The cryptomelane-type manganese oxide catalysts have been prepared by sol-gel method based on the redox reaction between potassium permanganate and glucose or oxalic acid. These catalysts belong to a class of porous manganese oxides known as octahedral molecular sieves (OMS). The SEM results indicated that the marked difference between the morphology of the cyptomelanes produced from glucose and oxalic acid. The glucose precursor produces cotton-shaped morphology, whereas the oxalic acid precursor leads to the formation of the disk-like appearances. The XRD results indicated that the glucose precursor produces more crystalline cryptomelane than that of oxalic acid. The effect of catalyst dosage on methyelene blue degradation was evaluated. Dye-decomposing activity was proportional to the amount of catalyst used, increasing of the catalyst amount leads to higher degradation of methyelene blue at short period of reaction. With different crystalline structures and morphology appearances of the cyptomelanes, however, the total degradation of methylene blue is relatively the same at 120 minute of reaction time with catalyst amount of 100 mg.
机译:通过基于高锰酸钾和葡萄糖或草酸之间的氧化还原反应,通过溶胶 - 凝胶法制备了加密蛋白型锰氧化物催化剂。这些催化剂属于一类被称为八面体分子筛(OMS)的多孔锰氧化物。 SEM结果表明,由葡萄糖和草酸产生的细胞蛋白的形态之间的显着差异。葡萄糖前体产生棉状形态,而草酸前体导致形成盘状外观。 XRD结果表明,葡萄糖前体产生比草酸更结晶更结束的胶囊。评价催化剂剂量对甲基蓝劣化的影响。染料分解活性与所用催化剂的量成比例,增加催化剂量导致在短时间内甲基烯蓝的较高降解。然而,具有不同的晶体结构和形态学的微细胞蛋白的外观,亚甲基蓝的总劣化在120分钟的反应时间与催化剂量为100mg。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号