Thin Wall Austempered Ductile Iron Connecting Rod for Lighter Automotive Component - Production of Thin Wall Ductile Iron Connecting Rod

机译:薄壁奥斯特普型球墨铸铁连杆连杆,用于较轻的汽车元件 - 生产薄壁球墨铸铁连杆连杆

获取原文

摘要

Lighter automotive components are produced to respond to global issue regarding energy. Lighter components can be achieved by replacing the material to those known as lighter material such as aluminium or applying thin wall casting technique. Lightweight automotive components will mean lower fuel consumption. Based on the success in making thin wall ductile iron plate (TWDI) with a thickness to 1 mm using a vertical casting, it encourages the implementation of the design to create lightweight automotive components. The design was applied to produce a thin wall two-cylinder engine ductile iron connecting rod which will be upgraded with austempering process. This connecting rod will be applied in Vespa PX150. The designs were simulated in Z-Cast simulation software and analyzed to determine the most optimum design. The chosen design was casted in a foundry to match the simulation. Evaluation of the characteristics will be run in the second stage of the research.
机译:制作更轻的汽车组件以应对有关能源的全局问题。通过将材料替换为称为较轻的材料,例如铝或施加薄壁铸造技术,可以通过更轻的部件来实现。轻量级汽车组件将意味着较低的燃料消耗。基于使用垂直铸造厚度为1毫米的薄壁球墨铸铁板(TWDI)的成功,它鼓励实施设计以创建轻量级的汽车组件。该设计应用于生产薄壁两缸发动机延展铁连杆连杆,该铁连杆连杆连接杆,其将以奥斯特型工艺升级。该连杆将应用于Vespa PX150。设计在Z-CAST仿真软件中进行了模拟,并分析以确定最佳设计。选择的设计在铸造中铸造以匹配模拟。对该特征的评估将在研究的第二阶段运行。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号