This research was conducted to study the effect of fly ash on alkaline activator ratio to the fly ash geopolymer artificial aggregate. The raw material used is fly ash, sodium silicate and sodium hydroxide. This research involves four different ratio of mix design which is 2.0, 2.5, 3.0 and 3.5 while ratio ofNaOH/NaSi_2O_3 is constant at 2.5. In this study, the molarity of NaOH is fix at 12M. The characterization of fly ash was done by X-Ray Fluorescence (XRF). The properties of fly ash geopolymer artificial aggregate then characterized by Aggregate Impact Value (AIV), and its microstructure been observed by Scanning Electron Microscope (SEM). Results show that, the sample with Fly Ash/Alkaline Activator 3.0 give the lowest percentage of AIV (19.6%) which denotes a high performance of aggregate in concrete field and also contribute to high performance of concrete while ratio 2.0 gives the highest percentage of AIV (25.19%). The tested results indicated that the significant potential of fly ash geopolymer aggregate as an alternative artificial aggregate in construction materials field.
机译:进行该研究以研究粉煤灰对粉煤灰地质聚合物人工骨料碱活化剂比的影响。使用的原料是飞灰,硅酸钠和氢氧化钠。该研究涉及与2.0,2.5,3.0和3.5的四种不同的混合设计比,而NAOH / NASI_2O_3的比例在2.5时恒定。在这项研究中,NaOH的摩尔性在12米处固定。粉煤灰的表征是通过X射线荧光(XRF)完成的。然后通过综合冲击值(AIV)表征粉煤灰地质聚合物人工骨料的性质,并通过扫描电子显微镜(SEM)观察其微观结构。结果表明,与粉煤灰/碱性活化剂,其表示在混凝土场聚集体的高性能的同时比2.0给出AIV的最高的百分比也有助于混凝土的高性能试样3.0给出AIV(19.6%)的比例最低(25.19%)。测试结果表明,粉煤灰地质聚合物骨料作为建筑材料领域中的替代人为骨料的显着潜力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号