摘要

The phosphating treatment coating is prepared on Mg-4.0Zn-1.0Sr-0.4Ca alloy surface,and the phosphating coating is consisted with HA and a small amount of calcium hydrogen phosphate hydrate.The hemolysis rate of both phosphated coating and uncoated samples is less than 5 %,showing that both have good hemolytic resistance which meet the requirements of use.It is found through the pathological studies that after implantation Mg-4.0Zn-1.0Sr-0.4Ca alloy for 30 days,for the leg muscle tissue,kidney tissue,liver tissue and bone tissues of rat the inflammation phenomenon is gradually recovered or completely recovered being passed the corrosion peak,while for the rat implanted the phosphating treatment alloy was in the acute stage of inflammation.After implantation Mg-4.0Zn-1.0Sr-0.4Ca alloy and the phosphating treatment alloy for 30 days,all of the brain tissue,myocardial tissue,lung tissue,intestinal tissue are unaffected.
机译:在Mg-4.0Zn-1.0SR-0.4CA合金表面上制备磷化处理涂层,磷化涂层和少量磷酸钙水合物组成。磷化涂层和未涂覆样品的溶血率较小比5%,表明均具有良好的溶血性,符合使用要求的溶血性。通过植入Mg-4.0zn-1.0SR-0.4Ca合金30天后的病理学研究发现,腿部肌肉组织,肾脏大鼠的组织,肝组织和骨组织炎症现象逐渐回收或完全回收通过腐蚀峰,而对于大鼠植入磷化处理合金在炎症的急性阶段。植入Mg-4.0zn-1.0sr -0.4CA合金和磷化处理合金30天,所有脑组织,心肌组织,肺组织,肠组织不受影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号