Study on the Causes and Prevention Measures of Shrinkage Defects of Heavy V-Belt Pulley in the Production

机译:生产重型V系皮带轮收缩缺陷的原因及预防措施研究

获取原文

摘要

Shrinkage cavity and shrinkage porosity, often occurring during the production of heavy v-belt pulley roughcast, may lead to the decrease of the pulley performance and further result in casting rejection. Therefore, it is necessary to study the causes and prevention measures of shrinkage defects of the casting. The material of V-belt pulley roughcast at issue is HT250 and it adopts resin sand casting process. With a large amount of practice in workshop and times of revision of the design of foundry technology, we have found that the shrinkage in the hot spot of heavy v-belt pulley roughcast can be reduced or even eliminated to fully meet the performance requirements with a moderate control of pouring temperature and speed, an optimized design of foundry technology, and a strict limitation of chemical composition. This finding will bring illumination to the production process of other heavy pulley roughcast.
机译:收缩腔和收缩孔隙率,通常发生在生产重型V形皮带轮粗糙期间,可能导致滑轮性能的降低,并进一步导致铸造排斥。因此,有必要研究铸造的收缩缺陷的原因和预防措施。 V-BIRT皮带轮粗糙的材料在问题上是HT250,它采用树脂砂铸造工艺。在车间和修订时期的铸造技术设计的大量实践中,我们发现,可以减少甚至消除重型V形皮带轮粗糙的热点的收缩,以完全满足性能要求适度控制浇注温度和速度,铸造技术优化设计,对化学成分的严格限制。这一发现将为其他重型滑轮粗糙的生产过程带来照明。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号