Formation and Prevention of Sliver Defects on the Surface of Cold-rolled Strip

机译:冷轧带材表面的形成和预防缺陷

获取原文

摘要

The feature and formation of and preventive measures against common black and bright slivers on the surface of cold-rolled strip are described. Research reveals that the formation of slivers is closely related to the processes of steel making and rolling as well as conditions of equipment in operation, and, in most cases, due to different factors affecting together. Only when the actual forming mechanism is made clear could effective measures be formulated.
机译:描述了对冷轧带材表面上共同的黑色和亮条的特征和形成和预防措施。研究表明,由于不同的因素在一起,钢制造和轧制的过程以及在大多数情况下,钢制造和轧制的过程密切相关。只有在明确的实际形成机制时,才能制定有效措施。