首页> 外文会议>Global Conference on Sustainable Manufacturing >Comparative Characterization of P91 and 10CrMo9-10 Creep Resistant Steel Welds
【24h】

Comparative Characterization of P91 and 10CrMo9-10 Creep Resistant Steel Welds

机译:P91和10CrMO9-10耐蠕变钢焊缝的比较表征

获取原文

摘要

P91 and 10CrMo9-10 creep resistant steels are critical to the performance of boiler tubes and power generating plants in general. Components made from these materials are mainly joined by welding. This paper reports on the comparative study of the effect of TIG and SMAW welding on the mechanical performance of P91 and 10CrMo9-10. TIG was used for root welding while SMAW was used for weld filling of V-butt joints. Specimens of the two alloys prepared using recommended welding procedures are evaluated using optical microscopy and Vickers micro hardness assessment. Some specimens were post weld heat treated while others were not. Post weld heat treated (PWHT) specimens exhibited similar properties as the corresponding base materials for both steels. TIG welding resulted in significant grain size reduction in both steels. PWHT produced more consistent grain structure, which is favorable.
机译:P91和10CRMO9-10蠕变抗性钢对锅炉管和发电厂的性能至关重要。由这些材料制成的部件主要通过焊接连接。本文报道了TIG和SMAW焊接对P91和10CrMO9-10的机械性能影响的比较研究。 TIG用于根焊接,而SMAW用于焊接V型对接接头。使用光学显微镜和维氏微型硬度评估评估使用推荐焊接程序制备的两种合金的标本。一些标本在焊接热处理,而其他标本则没有。焊接后焊接热处理(PWHT)标本表现出与两个钢的相应基材类似的性质。 TIG焊接导致两个钢的粒度大小减少。 PWHT生产了更一致的晶粒结构,这是有利的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号