The construction waste was processed into recycled aggregate to produce solid construction waste brick with grade of MU20. The preparation process of recycled aggregate and the optimal value of mass ratio of water to cement (water cement ratio) and mass ratio of recycled aggregate to cement was studied. The results shows that when the water cement ratio is 0.86 and the mass ratio of recycled aggregate to cement is 5.5 and the dosage of activator is 0.25% (mass fraction with recycled aggregate), the compressive strength of sample is 22.5 MPa and can be satisfied with the requirement of MU20 solid concrete brick.
机译:将建筑物废物加工成再循环骨料,以生产具有MU20等级的固体结构废砖。研究了再循环骨料的制备方法和水与水泥(水水泥比)和再循环骨料的质量比对水泥的质量比。结果表明,当水水泥比为0.86时,再循环聚集体与水泥的质量比为5.5并且活化剂的剂量为0.25%(带回收骨料的质量级分),样品的抗压强度为22.5MPa,可以满足随着MU20固体混凝土砖的要求。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号