This research of the PET/Nylon fabric pre-treatment by far-infrared and adding Methylenediphenylisocyanate(MDI) to 0%, 2%, 4%, 6% and 8%. According to fabric absorption medicament effect and bonding strength content analyzing. Heating 20 seconds, after stop 10 seconds and then heat 20 seconds and add 8% Methylenediphenylisocyanate(MDI) is the beast treatment, fabric-fabric adhesion strength is 16.73 kgf, fabric-rubber adhesion strength is 18.70 kgf, fabric-fabric and fabric-rubber adhesion strength that improve 54.6%, 69.6%.
机译:本型宠物/尼龙织物预处理的研究通过远红外线并加入甲基己酰基异氰酸酯(MDI)至0%,2%,4%,6%和8%。根据织物吸收药物效果和粘合强度含量分析。加热20秒,停止10秒后加热20秒并加入8%甲基己酰基异氰酸酯(MDI)是野兽处理,织物 - 织物粘合强度为16.73kgf,织物 - 橡胶粘合强度为18.70 kgf,织物 - 织物和织物 - 橡胶粘合强度,可提高54.6%,69.6%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号