Preparation and characteristics of chitin-gelatin composite film

机译:几丁质 - 明胶复合膜的制备及特征

获取原文

摘要

Using hydrogen peroxide as oxidant, the chitin has been oxidized under a certain conditions. And then the IR and SEM of product has been tested, and the results show that hydroxyl group can be transform carbonyl group. What's more, the oxidation reaction occurred not only in the surface of chitin, but also in its interior. Owing to the reaction of carbonyl group in the oxidation product, this chitin derivatives was applied to cross link with gelatin material, and the properties of modified gelatin film then has been tested. The results of Differential Scanning Calorimeter (DSC) show that the denaturation temperature of composite gelatin film has been enhanced to 109.8°C, and its swelling rate also has been slow, which ensure the stability as a kind of biomaterials, such as microcapsule and microspheres. And the time of native gelatin film achieving equilibrium swelling state is 9 minutes, and the time is 14 minutes for composite film, which means the oxidized chitin can delay the complete swelling rate. And the equilibrium swelling ratio of native gelatin film is larger than that of composite film. Therefore, the composite film will have a good prospects as a kind of potential biomedical.
机译:使用过氧化氢作为氧化剂,甲壳素在一定条件下被氧化。然后已经测试了产品的IR和SEM,结果表明羟基可以是转化羰基。更重要的是,氧化反应不仅发生在甲壳素的表面,也发生在其内部。由于羰基在氧化产物中的反应,将该丁蛋白衍生物施加与明胶材料的交联,然后测试改性明胶薄膜的性质。差分扫描量热计(DSC)的结果表明,复合明胶薄膜的变性温度已增强至109.8°C,其膨胀率也缓慢,这确保了一种生物材料(如微胶囊和微球)的稳定性。并且达到平衡肿胀状态的天然明胶膜的时间是9分钟,并且复合膜的时间为14分钟,这意味着氧化的甲壳素可以延迟完全溶胀率。天然明胶膜的平衡溶胀比大于复合膜的膨胀比。因此,复合薄膜将具有良好的前景作为一种潜在的生物医学。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号