A low refractive index, hard SiO_2 film was photochemically coated on the surface of slab laser head at room temperature by using silicone oil and a Xe_2 excimer lamp. Nd~+:glass slab laser produces high power laser because the light is amplified with a repeated total reflection in the laser medium. However, an evanescent wave arises on the total reflection interface, which causes a loss of the light energy. A low refractive index film 2 μm thick is, therefore, needed to prevent this problem. The vacuum vapor deposition method as a dry process and the spin-coating method as a wet process are generally used for making optical thin films. The former method can laminate a hard thin film, but requires temperatures above 500°C, and the thermal denaturation of the optical substrate is unavoidable. On the other hand, the latter method can form a low refractive index thin film, but the produced thin film has a poor adhesiveness and a low hardness. Besides, all these films are inferior in water resistance. We, therefore, formed a water-resistant, hard, and low refractive index protective coating directly on the laser glass surface at room temperature with photochemical reaction by the Xe2 excimer lamp.
机译:通过使用硅油和XE_2准分子灯,在室温下,低折射率,硬质SiO_2薄膜在室温下光学涂覆在平板激光头表面上。 ND〜+:玻璃板激光产生高功率激光,因为光在激光介质中的重复的全反射中放大。然而,在总反射界面上产生渐逝波,这导致光能的损失。因此,需要低折射率膜2μm厚的厚度以防止该问题。作为湿法的真空气相沉积方法作为干法和旋涂法,通常用于制造光学薄膜。前一种方法可以层压硬薄膜,但需要高于500℃的温度,并且光学基板的热变性是不可避免的。另一方面,后一种方法可以形成低折射率薄膜,但是产生的薄膜具有差的粘合性和低硬度。此外,所有这些薄膜都劣质耐水性。因此,我们在室温下直接在激光玻璃表面上直接形成防水,硬和低折射率保护涂层,通过XE2准分子灯的光化学反应。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号