Surface modification of precipitated calcium carbonate with self-made cationic styrene/acrylic emulsion was prepared and the experimental conditions of optimized modification parameters were defined by embedded ratio. The surface structure of modified precipitated calcium carbonate was characterized by FTIR. The result indicates that the maximum embedded ratio was 99% under the optimized modified conditions, which were as follows: temperature was 70 , pH was 9, the quality °C proportion between precipitated calcium carbonate and cationic styrene/acrylic ester copolymer was 75: 1. According to the spectra of FTIR, it was inferred that chemical binding and physical adsorption between surface modifiers and precipitated calcium carbonate had happened during the modification reaction. Using modified precipitated calcium carbonate as paper fillers, images of paper were observed by SEM (scanning electron microscope) and paper properties were tested. It was confirmed by SEM that distribution of modified precipitated calcium carbonate in paper was uniform and it was difficult to flocculate. Compared with unmodified precipitated calcium carbonate, the result indicates that PPF (paper perfect formation) value of papermaking added 35% modified precipitated calcium carbonate was low and the PPF value reduced after point of C6. Physical properties were improvements such as Z-direction force, bursting strength, tearing strength and tensile index increase10.51%, 74.3%, 38.7% and 64.6% respectively. Optical properties and ashing content of paper were also increased.
机译:制备沉淀碳酸钙的表面改性,制备了自制阳离子苯乙烯/丙烯酸乳液,并通过嵌入比率定义了优化改性参数的实验条件。改性沉淀的碳酸钙的表面结构通过FTIR表征。结果表明,在优化的修饰条件下,最大嵌入比例为99%,如下:温度为70,pH为9,沉淀的碳酸钙和阳离子苯乙烯/丙烯酸酯共聚物之间的质量°C比例为75:1 。根据FTIR的光谱,推断出在改性反应期间发生化学结合和表面改性剂和沉淀的碳酸钙之间的物理吸附。使用改性沉淀的碳酸钙作为纸填料,通过SEM(扫描电子显微镜)观察纸张的图像,并测试纸张性质。通过SEM通过SEM证实,所述修饰沉淀的碳酸钙的分布均匀,难以絮凝。与未经修改的沉淀碳酸钙相比,结果表明,PPF(纸张完美地层)造纸的价值添加了35%改性沉淀的碳酸钙,并且在C6点后PPF值降低。物理性质是Z方向力,爆破强度,撕裂强度和拉伸指数的改善,分别增加了10.51%,74.3%,38.7%和64.6%。纸张的光学性质和灰化含量也增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号