A range of hydrogels were prepared by solution polymerization of methacrylic acid, poly(ethyleneglycol) methyl ether methacrylate (M.W. 475 g/mol) and poly(ethyleneglycol) dimethacrylate (as the cross-linking, M.W. 550 or 875 g/mol) in various proportions. The effects of methacrylic acid/ poly(ethyleneglycol) methyl ether methacylate concentration ratios as well as cross-linking concentration in the degree of swelling as a function of the media pH were studied. Reversibility of the swelling process was confirmed. Degradation in the system described previously was introduced using a hydrolytically labile diacrylate cross-linker (A-PLA-PEG-PLA-A) instead of the poly(ethyleneglyco) dimethacrylates. The degrees of swelling and degradation rates at different pH were studied. Hydrolytically degradable polymers that respond to pH stimuli to activate the swelling and decomposition process were developed. Multiple interrelated control parameters dictated by the synthetic recipe were studied and are available to separately control swelling and degradation rates of these novel polymers.
机译:通过甲基丙烯酸的溶液聚合,聚(乙二醇)甲基醚甲基丙烯酸酯(Mw 475g / mol)和聚(乙二醇)二甲基丙烯酸酯(作为交联,MW 550或875g / mol)的溶液聚合制备了一系列水凝胶。比例。研究了甲基丙烯酸/聚(乙二醇)甲基醚甲酯浓度比以及作为培养基pH的函数的溶胀程度的交联浓度的影响。确认了膨胀过程的可逆性。使用水解不稳定的二丙烯酸酯交联剂(A-PLA-PEG-PLA-A)代替聚(乙醇)二甲基丙烯酸酯来引入先前描述的系统中的降解。研究了不同pH的肿胀程度和降解率。开发出响应pH刺激以激活溶胀和分解过程的水解可降解聚合物。研究了合成配方所示的多个相互关联的控制参数,可用于单独控制这些新型聚合物的溶胀和降解速率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号