Mould fluxes play an important part in continuous casting. They must lubricate the steel shel and provide the right level of horizontal heat transfer in order to avoid both longitudinal cracking and sticker breakouts. Powder consumption (Q_s in kg flux/m~2 of mould) is a measure of the lubrication supplied by the mould flux. Plant data for billet - , bloom-, slab-and thin slab- casting from steelworks all over the world have been analysed. It is shown that Q_s is a sensitive function of the parameter, R (ratio of surface area/volume of the mould) which is a function of the mould dimensions. The melting rate of the flux must satisfy the demand for molten slag and it is shown that the hierarchy of the parameter (percent C/R) is in the order of slabs and thin slabs>blooms>billets. The horizontal heat transfer is controlled by the thickness and the crystallinity of the solid slag film in the mould/strand gap. The thickness of the slag film is partially determined by the reak (or solidification) temperature; plots of recommended break temperature as functions of viscosity and casting speed are given for the optimum casting of different steel grades.
机译:模具助熔剂在连续铸造中起重要作用。它们必须润滑钢架并提供水平传热的正确水平,以避免纵向开裂和贴纸突出。粉末消耗(QG助焊剂/ M〜2中的Q_S)是模具通量提供的润滑的量度。分析了钢结构的植物数据 - 来自世界各地的钢厂的钢结构。结果表明,Q_S是参数的敏感函数,R(模具的表面积/体积的比率),其是模具尺寸的函数。通量的熔化速率必须满足对熔渣的需求,并显示参数的等级(C / R)的等级是平板和薄板条>盛开>坯料的顺序。水平传热由模具/股线间隙中的固体渣膜的厚度和结晶度控制。炉渣薄膜的厚度部分地由锋利(或凝固)温度部分确定;推荐的断裂温度作为粘度和铸造速度的函数的曲线,用于不同钢等级的最佳铸造。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号