Preparation of Calcium Oxide/Zeolite Nanocomposite and its Application to Improve the Quality of Patchouli Oil

机译:氧化钙/沸石纳米复合材料的制备及其应用提高广藿香油的质量

获取原文

摘要

The synthesis of CaO/zeolite nanocomposite as a highly active and effective adsorbent for patchouli oil purification has been developed. This research aims to improve the quality of patchouli oil by synthesizing CaO/zeolite nanocomposites using a solid-state mixing method. The used mass ratios of zeolite:CaO were 0:100, 20:80, 40:60, 60:40, 80:20 and 100:0 (w/w), then nanocomposites with various zeolite-to-CaO ratios were then calcined at various temperature of 300°C, 400°C and 500°C. The zeolite, CaO and nanocomposites were characterized by using the Fourier-transform infrared (FTIR), X-ray fluorescence spectrometer (XRF) and surface area analyzer (SAA). The nanocomposites were then applied to patchouli oil and the assessment results of physical and chemical properties of patchouli oil were determined according to Indonesian National Standard (SNI) 06-2385-2006. After patchouli oil purification using ZECA nanocomposite, the acid number decreased from 5.42 to 0.39 mg KOH/g oil, the patchouli alcohol (PA) content increased from 33.08 to 34.27% and the Fe level decreased from 1.39 to 0.31 ppm.
机译:已经开发了CaO /沸石纳米复合材料的合成,作为菠萝油净化的高活性和有效的吸附剂。该研究旨在通过使用固态混合方法合成CaO /沸石纳米复合材料来改善菠萝油的质量。沸石的使用量率:CaO为0:100,20:80,40:60,60:40,80:20和100:0(w / w),然后是具有各种沸石 - 至Cao比率的纳米复合材料在300℃,400℃和500℃的各种温度下煅烧。通过使用傅里叶变换红外(FTIR),X射线荧光光谱仪(XRF)和表面积分析仪(SAA)来表征沸石,CAO和纳米复合材料。然后将纳米复合材料施用于爆炸性油,根据印度尼西亚国家标准(SNI)06-2385-2006确定了PAPPOULI油的物理和化学性质的评估结果。在采用Zeca纳米复合材料进行洪水净化后,酸值从5.42减少到0.39mg KOH / G油,PAPPOULI醇(PA)含量从33.08增加到34.27%,并且FE水平从1.39降至0.31 ppm。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号