It was tested the strength and wear value of recycled aggregate concrete mixing fly ash, slag, silica fume and double-mixture or three-mixture in deferent age. The results show that the wear value of recycled aggregate concrete mixing 30% fly ash is more than reference concrete at 3 days, but can improve final wear-resisting property significantly. The wear value of recycled aggregate concrete mixing 30% double-mixture of fly ash and silica fume is much lower than reference concrete at 3 days, and improve early wear-resisting property significantly. The flexural strength of the concrete is 4.26 MPa at 3 days, which can satisfy the traffic requirement. The wear value of recycled aggregate concrete mixing 30% three-mixture of fly ash, slag and silica fume is lower than reference concrete at 3 days, but the declining rate is not significant. It investigates mechanics of double-mixture technique which improves wear-resisting property at the same time.
机译:测试了再生骨料混凝土混合粉煤灰,炉渣,二氧化硅烟气和双混合物或三种混合物的强度和磨损值。结果表明,回收骨料混凝土混合30%粉煤灰的磨损值在3天内比参考混凝土更大,但可以显着提高最终耐磨性。再循环骨料混凝土混合的磨损值与粉煤灰和二氧化硅烟气的30%双混合物在3天内比参考混凝土低得多,并显着提高早期耐磨性。混凝土的抗弯强度为3天,3天为4.26MPa,可以满足交通要求。再循环骨料混凝土混合的磨损值30%三种混合物的粉煤灰,炉渣和二氧化硅烟雾在3天的参照混凝土中低于参考混凝土,但下降率并不显着。它研究了双混合技术的机制同时改善耐磨性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号