Thermal Behaviour of Materials Based on Calcium Sulfo-aluminate Cement

机译:基于磺铝铝酸钙水泥的材料的热行为

获取原文

摘要

This paper deals with the thermal behaviour (up to 1,250°C) of different materials based on calcium sulfo-aluminate cement: cement pastes, standard mortars and lightweight mortars. The behaviour of calcium sulfo- aluminate cement pastes containing varying amounts of phosphogypsum (0 to 40%) and two types of calcium aluminate clinker was first investigated. The best behaviour was shown by the pure clinker and the cement containing 20% phosphogypsum. Then, standard mortars containing siliceous sand, and either pure clinker or cement containing 20% phosphogypsum were heated up to 1250°C. They remained intact. Finally, lightweight materials using calcium sulfo-aluminate cement and either perlite or vermiculite were investigated. All samples containing vermiculite remained intact up to 1250°C.^
机译:本文涉及基于氧化钙 - 铝酸钙水泥的不同材料的热行为(最多1,250°C):水泥浆料,标准砂浆和轻质砂浆。首先研究含有不同量的磷酸糖磷膏(0至40%)和两种类型的铝酸钙熟料的钙磺酸钙水泥浆料的行为。纯熟料和含有20%磷蛋白的水泥显示的最佳行为。然后,含有硅子砂的标准砂浆,含有20%磷酸缺口的纯熟料或水泥被加热至1250℃。他们保持完整。最后,研究了使用磺基铝酸钙水泥和珍珠岩或蛭石的轻质材料。含有蛭石的所有样品仍然完好无化,最高可达1250℃^

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号