The change in the morphology of the dendritic primary α -Al crystals heated at the semi-solid temperatures was examined in Al-7%Si-3%Cu alloy containing 0.1~1.0% Fe. Dendritic α -Al crystals, which were refined by Ti-B addition and solidified with higher cooling rate than 10K/s, spheroidize only by heating up to the semi-solid state without stirring. The size of the spheroidized primary α -Al crystals is about 100 μ m in diameter. The elongation of the as-semi-solid cast materials is superior to that of the conventional gravity diecast materials, causing 9% of elongation even in the alloy containing 1% Fe. The tensile properties of the alloy materials containing small amount of Mn are further improved by changing morphology of Fe intermetallic compounds from needle-like form to Chinese script one.
机译:在含0.1〜1.0%Fe的Al-7%Si-3%Cu合金中检查在半固体温度下加热的树突式初级α-产物晶体的形态的变化。树枝状α-产物晶体,其通过Ti-b加入并以比10k / s更高的冷却速率固化,仅通过在不搅拌的情况下加热到半固态的球形。球化初级α-晶体的尺寸直径为约100μm。半固态铸造材料的伸长率优于传统重力压铸材料,即使在含有1%Fe的合金中,也导致伸长率的9%。通过从针状形式改变Fe金属间化合物的形态,进一步提高了含有少量Mn的合金材料的拉伸性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号