The possibility of producing iron and silicon-coagulant-fiocculant for purification of waste water was shown. The electric steel melting slag JSC "OMK-Steel" has been used as the starting material, in which the content of iron oxide to 25.8% and silicon dioxide is 17.6%. The optimal parameters of slag hydrochloric opening were as follows: the modification time at T = 40 °C - 1 hour, the concentration of hydrochloric acid - 1.5 N, the ratio of the solid and liquid phases of S : L = 1 : 10. In these settings the concentration of hydrosilicic acid (for silicon) will be 1532 mg/1; the concentration of iron - 1250 mg/1 has a lower concentration of silicic acid in the production of the solution with increasing temperature and time of exposure. This paper examined the chemical aspects of the process of obtaining the new iron- containing coagulant- flocculant based on electric furnace slag. The results can be used to produce coagulants and flocculants using industrial waste.
机译:显示了生产用于净化废水的铁和硅凝结剂絮凝​​剂的可能性。电工钢渣JSC“ OMK-Steel”已被用作起始原料,其中氧化铁含量为25.8%,二氧化硅含量为17.6%。炉渣盐酸盐开孔的最佳参数如下:在T = 40°C的改性时间-1小时,盐酸的浓度-1.5 N,固液比S:L = 1:10。在这些设置下,氢硅酸(硅)的浓度将为1532 mg / 1。随着温度和暴露时间的增加,溶液生产中铁的浓度-1250 mg / 1具有较低的硅酸浓度。本文研究了基于电炉渣的新型含铁凝结剂-絮凝剂的制备过程的化学方面。该结果可用于利用工业废料生产凝结剂和絮凝剂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号