This paper presents an experimental investigation on the failure modes of glass fiber reinforced 2D woven fabric with ladder splicing laminate composites.On the basis of [0/0/+45/90/-45/90]s ply sequence,six kinds of laminated performs with different splicing interval lengths which were 4mm,8mm,12mm respectively and two different splicing shape which were ladder splicing and double vertical line splicing,and a kind of laminated perform with continuous laminates of 2D glass fiber woven fabric were made.By means of RTM molding technology,the technological parameters of RTM processing were designed as follows:injection temperature was 25°C,injection duration time was 180rmin and injection pressure was 0.4MPa,the epoxy resin based 2D glass fiber woven fabric RTM laminated specimen were prepared.According to the GB/T 1447-2005 and GB/T 1449-2005standard test method,the failure modes of 2D glass fiber woven fabric laminated RTM specimen were tested.Results show that the failure modes of laminate composites manifest as rapid damage in the form of line inlay mode and wedge shape mode at 4mm interval length condition,and accumulating failure in the form of inlay layer slippage-fiber pulled out mode and fiber fracture-splicing layer deboning mode at 12mm interval length.Otherwise,all fracture position of splicing laminates occurs at the site of splicing line because of the concentration of tensile stress.
机译:本文对梯形拼接层压复合材料玻璃纤维增​​强2D机织物的破坏模式进行了实验研究。在[0/0 / + 45/90 / -45 / 90] s层序的基础上,对六种层压材料进行了研究。分别以4mm,8mm,12mm的不同拼接间隔长度和梯形拼接和双垂直线拼接两种不同的拼接形状进行拼接,制成一种具有连续2D玻璃纤维织物的叠层制品。 RTM成型技术,RTM加工的工艺参数设计如下:注射温度为25°C,注射持续时间为180rmin,注射压力为0.4MPa,制备了环氧树脂基2D玻璃纤维机织RTM层压样品。根据GB / T 1447-2005和GB / T 1449-2005标准测试方法,测试了2D玻璃纤维织物层压RTM标本的失效模式。结果表明,lami的失效模式天然复合材料在4mm间隔长度条件下表现为线镶嵌模式和楔形模式的快速破坏,在12mm间隔长度条件下表现为镶嵌层滑移-纤维拉出模式和纤维断裂-接缝层剥离模式的累积破坏否则,由于拉伸应力的集中,拼接层压板的所有断裂位置都发生在拼接线的位置。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号