Effects on Impact-Echo Signals Caused by Adjacent Steel Reinforcing Bars and Defects in Lap-Splice Regions: Experimental Study

机译:钢筋加固杆和液体劈开杆和缺陷引起的冲击回波信号的影响:实验研究

获取原文

摘要

Previous studies have identified the impact-echo method as a viable technique for detecting defects around steel reinforcing bars in reinforced concrete (RC) members. Defects can form around reinforcement as a result of corrosion, alkali-silica reactions, delayed ettringite formation, freezing and thawing, and other deterioration mechanisms. This paper investigates the feasibility of using impact echo testing on RC members to evaluate defects in lap-splice regions. In lapped bars challenges exist because adjacent bars may have different defect conditions. A small-scale experimental setup for making this determination is designed to replicate field conditions. Variables in the experiment include defect thickness and defect length. Impact-echo results from the small-scale experimental design are presented to determine if impact-echo testing can be used to identify the presence of defects at the steel concrete interface in specimens containing adjacent steel reinforcing bars.
机译:以前的研究已经确定了冲击回波方法作为用于检测钢筋混凝土(RC)构件中钢筋钢筋的缺陷的可行技术。由于腐蚀,碱二氧化硅反应,延迟的eDtringite形成,冷冻和解冻等缺陷,缺陷可以形成抗缺陷,以及其他劣化机构。本文研究了利用影响回波测试对RC成员的可行性来评估液体剪接区域的缺陷。在拉盖的条形栏中存在挑战,因为相邻的棒可能具有不同的缺陷条件。用于使该确定的小规模实验设置旨在复制现场条件。实验中的变量包括缺陷厚度和缺陷长度。提出了小规模实验设计的冲击回波结果以确定是否可以使用冲击回波测试来识别含有相邻钢筋棒的样本中的钢混凝土界面处的缺陷。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号