In the late 80's and early 90's the research community generated substantial test data that showed a reduction in fatigue life (Stress versus cycle, i.e., S-N mehtod) due to environmental effects from pure, high oxyfgenated water. Previous to the S-N testing, the research community had shown a substantial increase in crack growth rates (called EAC - environmental assisted cracking) from the same environment. The environment is that of the primary water in nuclear power plants. After a number of PVRC meeting discussions, a project was initiated in 1991 with a team called the Steering Committee For Cyclic Life for Environmental Effects (CLEE). The scope of the committee was to study the impact of the environmetnal test data on current ASME Code, Section XI rules and to report findings and make recommendations to the ASME BNCS (Board on Nuclear Codes and Standard).
机译:在80年代末和90年代初,研究团体生成了大量测试数据,这些数据表明,由于纯净的高含氧量水对环境的影响,疲劳寿命(应力与周期,即S-N甲基苯丙胺)降低。在进行S-N测试之前,研究团体已经表明,同一环境下的裂纹增长率(称为EAC-环境辅助裂纹)大幅增加。环境是核电厂的主要水的环境。经过多次PVRC会议讨论后,1991年与一个名为“影响环境的循环生命指导委员会”(CLEE)的团队启动了一个项目。该委员会的职责是研究环境测试数据对当前的ASME规则第XI条规则的影响,并向ASME BNCS(核法规和标准委员会)报告调查结果并提出建议。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号