Break operation studies have been conducted upon silver metal-oxide (Ag/MeO) contact materials under DC conditions between 1-16 Amps. The materials used in this study are Ag/CdO and Ag/SnO/sub 2/ typically used in low voltage switching. The apparatus used in the study has been previous presented and allows contact materials to be continually tested with fully controlled break velocity. The results presented include erosion data in terms of mass transfer and surface analysis using scanning electron microscopy. Scanning electron micrographs reveal distinct structures and areas on the contact surface. Elemental analyses (EDS) was also conducted which show migration of metal species in the Ag/MeO, with various current loads. It is shown that the type of metal-oxide used in the contact significantly influences the arc and erosion characteristics on break operations. Contacts have been shown to exhibit different erosion/deposition characteristics at particular current on break operations. Erosion and deposition of the contacts on break have been related to two parameters: arc energy and arc duration.
机译:已经在1-16安培的直流条件下对金属银氧化物(Ag / MeO)接触材料进行了断路操作研究。本研究中使用的材料通常为低压开关中使用的Ag / CdO和Ag / SnO / sub 2 /。该研究中使用的设备已在前面介绍过,可以在完全受控的断裂速度下连续测试接触材料。给出的结果包括在传质和使用扫描电子显微镜进行表面分析方面的腐蚀数据。扫描电子显微照片揭示了接触表面上不同的结构和区域。还进行了元素分析(EDS),显示了在各种电流负载下,金属物种在Ag / MeO中的迁移。结果表明,触点中使用的金属氧化物的类型会显着影响断开操作时的电弧和腐蚀特性。已经显示,在断开操作的特定电流下,接触件表现出不同的腐蚀/沉积特性。触头的腐蚀和沉积与两个参数有关:电弧能量和电弧持续时间。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号