Thixoforming of Wrought Aluminum Alloy 1973

机译:变形铝合金的触变性1973

获取原文

摘要

In this paper, the microstructure and mechanical properties of thixoformed 1973 (AlZn5.5Mg2.4Cul.7Zr) wrought aluminium alloy were investigated. A cooling slope was used to produce non-dendritic billets. Thixoforming process parameters were determined as follows: die temperature of 250 °C, feedstock temperature of 600 - 605 °C, punch velocity of 7 mm/s. Mechanical properties of thixoformed with ultimate strength of 461 MPa and elongation of 3,1 % in the T2 condition. The lower properties of the thixoformed material are mainly associated with porosity.
机译:研究了触变成形1973(AlZn5.5Mg2.4Cul.7Zr)变形铝合金的组织和力学性能。使用冷却斜率生产非树枝状坯料。触变成型工艺参数的确定如下:模头温度为250°C,原料温度为600-605°C,冲头速度为7 mm / s。触变成形的机械性能在T2条件下具有461 MPa的极限强度和3.1%的伸长率。触变材料的较低性能主要与孔隙率有关。