Our present fluoroalkyl end-capped DOBAA oligomer/silica nanocomposites, in which the oligomer contents are 18 ~ 72 %, were found to exhibit no weight loss even at 800 °C, although the corresponding oligomer decomposed completely around 540 °C. In contrast, sub-micrometer size-controlled Rp-(DOBAA)_n-R_F/silica composites (the oligomer content: 24 %) exhibited a clear weight loss characteristic at 800 °C.
机译:我们目前的氟代烷基端封端的DOBAA低聚物/二氧化硅纳米复合材料,其中寡聚物含量为18〜72%,甚至在800℃下也没有减肥,尽管相应的低聚物完全分解在540℃约为540℃。相反,亚微米尺寸控制的RP-(DOBAA)_N-R_F /二氧化硅复合材料(低聚物含量:24%)在800℃下表现出清晰的体重减轻特性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号