Method of equivalent research of typical automotive parts

机译:典型汽车零部件的等效研究方法

获取原文

摘要

The sample corrosion shape and appearance are compared between vehicle accelerated corrosion test and laboratory accelerated corrosion test. An equivalent relationship between laboratory accelerated corrosion and actual service condition is obtained on the basis of the research of distribution characteristics for two corrosion damage. The calculation indicates that this relationship of typical component: y = 32.86 e0.5x (where, y is time of laboratory accelerated corrosion, x is time of actual service condition), thereby laying a foundation for anti-corrosion design and coating selection.
机译:在车辆加速腐蚀试验和实验室加速腐蚀试验之间比较了样品腐蚀的形状和外观。在研究两种腐蚀损伤的分布特征的基础上,得出了实验室加速腐蚀与实际使用条件之间的等效关系。计算表明,这种典型成分之间的关​​系为:y = 32.86 e 0.5x (其中y是实验室加速腐蚀的时间,x是实际使用条件的时间),从而为防腐蚀奠定了基础。腐蚀设计和涂层选择。