A material with perovskite structure, lanthanum strontium cobaltite ferrite, La_(0.6)Sr_(0.4)Co_(0.2)Fe_(0.8)O_(3-δ)(LSCF6428) has gained attention as a cathode component for intermediate to low temperature solid oxide fuel cells (IT-LTSOFCs). In this study, LSCF6428 films were developed via the electrophoretic deposition (EPD) technique with the use of an aqueous solvent. 1 wt% of LSCF6428 was suspended in deionised water for the preparation of the EPD suspensions. The EPD process at applied voltages of between 3 to 7 V and deposition times of 3 to 10 minutes has been found to be able to deposit LSCF6428 films. Additionally, the use of additives such as starch and polymethyl methacrylate (PMMA) was found to effectively improve the quality of the deposited films. It is concluded that the applied voltage, deposition time and the addition of additives play important roles that affect the morphology and weight of the deposited films.
机译:具有钙钛矿结构的镧锶钴铁氧体La_(0.6)Sr_(0.4)Co_(0.2)Fe_(0.8)O_(3-δ)(LSCF6428)作为中低温固体氧化物的阴极组分备受关注燃料电池(IT-LTSOFC)。在这项研究中,LSCF6428膜是通过使用水性溶剂通过电泳沉积(EPD)技术开发的。将1重量%的LSCF6428悬浮在去离子水中以制备EPD悬浮液。已经发现,在3至7 V的施加电压和3至10分钟的沉积时间下进行的EPD工艺能够沉积LSCF6428膜。另外,发现使用添加剂例如淀粉和聚甲基丙烯酸甲酯(PMMA)可以有效地改善沉积膜的质量。结论是施加的电压,沉积时间和添加剂的添加对影响沉积膜的形态和重量具有重要作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号