Effect of using a hot-press to suppress surface checks in sugi boxed heart square timbers during the drying process

机译:使用热压机的效果抑制干燥过程中Sugi盒装心脏方形木材表面检查的影响

获取原文

摘要

The high temperature drying method has become popular for drying sugi (Cryptomeriajaponica D.Don) boxed heart square timbers in Japan because it shortens the drying time and suppresses surface checks. However, it is well known that internal cracks and surface discoloration often occur in sugi boxed heart square timbers during the drying process. We investigated the effect of using a hot-press for suppressing surface checks in sugi boxed heart square timbers during the drying process. That is to say, the objective of this study was to reduce the damage of timbers during the drying process by shortening the high temperature drying time. The treatment for suppressing surface checks in timber is to form a surface drying set in it. This report presents the effect of using a hot-press for the formation of a surface drying set in sugi boxed heart square timbers. The results of this study are summarized below. (1) The inside of the sugi boxed heart square timbers showed almost no drying with this surface treatment. (2) Surface drying of the sugi boxed heart square timbers could be carried out uniformly with 30 min of hot-pressing with hardly any influence from the wide variations in moisture content. However, there was no good progress in drying over the 2nd layer under any of the test conditions. (3) Higher plate heating temperatures resulted in deeper heating in the sugi boxed heart square timbers. (4) In this surface treatment, the drying set was formed in the 1st layer under each test condition. However, in the 2nd and 3rd layers, the drying set was hardly formed. (5) In this study, two types of plates were used: a flat plate with a smooth surface and a slit plate with grooves cut into the surface to make it easier for it to release vapor. However in these results, the effect of creating slits was not apparent.
机译:因为它缩短了干燥时间和禁止显示表面检查高温干燥方法已成为流行的烘干杉(Cryptomeriajaponica D.Don)盒装心脏方形横梁在日本。然而,众所周知的是,内部裂纹和表面变色在干燥过程中经常会出现在杉盒装心脏方形横梁。我们调查使用热压对在干燥过程期间抑制杉盒装心脏方形横梁表面检查的效果。也就是说,本研究的目的是通过缩短高温干燥时间,以减少在干燥过程中木材的损坏。在木材表面抑制检查处理是形成在它的表面干燥组。这份报告给出了使用热压在杉盒装心脏方形横梁形成了表面干燥组的效果。这项研究的结果总结如下。 (1)杉盒装心脏方形横梁的内部显示出与该表面处理几乎没有干燥。 (2)盒装杉心脏方形横梁的表面干燥,可以用30分钟均匀地进行热压,几乎没有从在水分含量的大范围变化的任何影响。然而,有在任何在测试条件下干燥在所述第二层中没有良好的进展。 (3)较高的板的加热温度导致了杉盒装心脏方形横梁更深加热。 (4)在该表面处理,形成在每个测试条件下的第一层干燥集。然而,在第二和第三层,几乎没有形成所述干燥组。 (5)在本研究中,使用了两种类型的板:平板具有光滑表面,并与切入表面的凹槽的狭缝板,使其更容易为它释放蒸汽。然而,在这些成绩,创造缝隙的效果并不明显。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号