The extraction of titanium from the Ti-enriched product which was prepared from Ti-bearing blast furnace slag by alkali roasting and water leaching, was investigated by dilute sulfuric acid leaching. The effects of sulfuric acid mass fraction, the ratio of acid to slag, reaction temperature and time on the extraction rate of titanium were studied in this paper. The results show that titanium recovery of 92.62 pct was obtained under the conditions of sulfuric acid mass fraction of 50 pct, ratio of acid to slag of 1.5:1, reaction temperature of 160°C and reaction time of 2.5 hours. The kinetic study indicates that the acid leaching reaction was controlled by the rate of diffusion, and kinetics equation of drozdov can be described the acid leaching reaction.
机译:通过稀硫酸浸出研究了由碱焙烧和水浸出的Ti富含Ti-uck Ellow炉渣制备的Ti富含Ti富炉炉渣的富含Ti富含Ti富含炉渣的钛的提取。本文研究了硫酸质量级分,酸与炉渣的比例,反应温度和时间对钛的提取率的影响。结果表明,在50pct的硫酸质量分数的条件下获得了92.62pct的钛回收率,酸与炉渣的比例为1.5:1,反应温度为160℃,反应时间为2.5小时。动力学研究表明,通过扩散速率控制酸浸出反应,并且Drozdov的动力学方程可以描述酸浸出反应。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号