Take Pinus massoniana and Pinus sylvestris vat. mongolica as the material of experiment, Rapeseed Oil as the medium of conducting the treatment process of wood oil heat-to-charring wood. The results show that: in the initial heat treatment, the initial moisture content of wood should be less than 10%, then rise the temperature of HTF to about 100℃ rapidly at the speed of 10-13 ℃/h, then slowly increase to 130 ℃ at the speed of 3-5℃/h to process high temperature wood drying to dry wood to absolute dry. After that, rise the temperature to between 195-220℃ at the speed of 12-16℃/h to deal with charring wood. The time of treatment is determined by the need of wood species, thickness and usage, for the general it is 2-4h. After the carbonization lumber size stable, does not have the dehiscence and the distortion occurrence.u0000 deal
机译:以马尾松和樟子松大桶为例。蒙古油为实验材料,菜籽油为进行木油热合木处理工艺的介质。结果表明:在初始热处理中,木材的初始含水量应小于10%,然后以10-13℃/ h的速度将HTF的温度迅速升高至约100℃,然后缓慢升高至以3-5℃/ h的速度在130℃下进行高温木材干燥,使木材干燥至绝对干燥。之后,以12-16℃/ h的速度将温度升至195-220℃以处理炭化木材。处理时间取决于木材种类,厚度和用量的需要,通常为2-4小时。碳化木材尺寸稳定后,不开裂和变形发生。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号