Preparation of Sliver Nanoparticles by Liquid Chemical Reduction Method

机译:液相化学还原法制备纳米银

获取原文
获取原文并翻译 | 示例

摘要

The development of printing electronics technology promotes the application of conductive ink, and nano-silver conductive ink is a hot research. Sliver particles are the main conductive component in conductive ink, so nano-silver particles are very important for the ink conductivity. In this paper, silver nanoparticles were reduced from silver nitrate solution by liquid chemical reduction method, with Sodium hypophosphite as reductant, PVP as surface-protection reagent, and sodium hexametaphosphate as dispersant. Orthogonal test with 4 factors and 3 levels is designed in which the effect of reducing agent dosage, protective agent dosage, dispersant content and reaction temperature on the nano-particle size and morphology of silver is investigated. The size distribution of nano-silver powder is measured by nano-size potential analyzer, and the morphology of silver particles is characterized with the SEM. The experiment results showed that the minimum average size of sliver particles can reach 23.87nm, and the dispersed spherical nano-particles with the average size is about 60nm can be obtained.
机译:印刷电子技术的发展促进了导电油墨的应用,而纳米银导电油墨是一个热门研究。银粒子是导电油墨中的主要导电成分,因此纳米银粒子对于油墨的导电性非常重要。本文采用液相化学还原法,以次磷酸钠为还原剂,PVP为表面保护剂,六偏磷酸钠为分散剂,通过液相化学还原法从硝酸银溶液中还原出银纳米颗粒。设计了4个因子,3个水平的正交试验,研究了还原剂用量,保护剂用量,分散剂含量和反应温度对银的纳米粒径和形貌的影响。用纳米电势分析仪测量纳米银粉的粒度分布,并用SEM表征银颗粒的形貌。实验结果表明,条状粒子的最小平均粒径可达23.87nm,平均粒径约为60nm。

著录项

  • 来源
  • 会议地点 Minneapolis MN(US);Minneapolis MN(US);Minneapolis MN(US);Minneapolis MN(US)
  • 作者单位

    State Key Laboratory of Pulp and Paper Engineering, South China University of Technology, Guangzhou, 510641, China;

    State Key Laboratory of Pulp and Paper Engineering, South China University of Technology, Guangzhou, 510641, China;

    State Key Laboratory of Pulp and Paper Engineering, South China University of Technology, Guangzhou, 510641, China;

    State Key Laboratory of Pulp and Paper Engineering, South China University of Technology, Guangzhou, 510641, China;

  • 会议组织
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类 数字印刷;
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号