Grain refinement effect of La_2(CO_3)_3 on AZ91 magnesium alloy

机译:La_2(CO_3)_3对AZ91镁合金的晶粒细化作用

获取原文
获取原文并翻译 | 示例

摘要

The La_2(CO_3)_3 addition makes the grain of AZ91 alloy be refined obviously. The average primary dendrite size of the alloy decreases from 150 to 50 μm. The microstructure of typical dendrite turns into the equal-axed grain with the addition of 2.5 wt. % La_2(CO_3)_3 refiner. The mechanical properties tests indicate that the tensile strength and especially elongation of the alloys are improved with the addition of La_2( CO_3)_3 and their maximum enhancing rates based on the La2(CO_3)_3-free AZ91 alloy are 26% and 5.2 times at 2.5 wt. % La_2(CO_3)_3 refiner respectively.
机译:La_2(CO_3)_3的添加使AZ91合金的晶粒明显细化。合金的平均一次枝晶尺寸从150微米减小到50微米。添加2.5 wt。%的枝晶后,典型的枝晶的微观结构变为等轴晶。 %La_2(CO_3)_3磨浆机。力学性能测试表明,加入La_2(CO_3)_3可以提高合金的拉伸强度,尤其是延伸率,基于不含La2(CO_3)_3-的AZ91合金,其最大增强速率为26%和5.2倍。 2.5重量分别为%La_2(CO_3)_3磨浆机。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号