This paper reported the analysis results from the SEM (scanning electron microscope)and AES (Auger Electron Spectroscopy) of HIP(hot isostatically pressed)stellite 12 in a 3.5% NaCl liquid medium.The aim of the paper is to determine thickness and the composition of the passive film formed at different HIP temperatures, different primary power size and link that to the corrosion properties.It has been shown that the alloy passivate spontaneously in air resulting in the formation of a thin oxide film comprising Cr and Co.film thickness is from 30 ~39nm.Electrochemical oxidation at different HIP temperature results in formation of complex layer, the composition and thickness of which depends on the HIP temperature and primary power size.Cl was detected in the surface layer ,but did not permeate in passive film, O enriched in 1.5nm under surface layer.This paper mainly introduced the influence of HIP temperature for space limitation.
机译:本文报道了在3.5%NaCl液体介质中,HIP(热等静压)Stellite 12的SEM(扫描电子显微镜)和AES(俄歇电子能谱)分析结果。本文的目的是确定厚度和组成在不同的HIP温度,不同的初次功率尺寸以及与腐蚀性能相关的钝化膜中发现,该合金会在空气中自发钝化,从而形成包含Cr和Co的氧化膜。在30〜39nm范围内。在不同的HIP温度下进行电化学氧化会形成复杂的层,其组成和厚度取决于HIP温度和一次功率的大小。在表面层中检测到Cl,但没有渗透到钝化膜中, O在表层下富集1.5nm。本文主要介绍了HIP温度对空间限制的影响。

著录项

  • 来源
  • 会议地点 Beijing(CN)
  • 作者单位

    Advanced Technology Materials Co., Ltd., Beijing 100086, China;

    Engineering and Technology Research Center of Hot Isostatic Pressing, Zhuozhou Hebei 072750, China;

    Advanced Technology Materials Co., Ltd., Beijing 100086, China;

    Engineering and Technology Research Center of Refractory Materials, Beijing 100083, China;

    Advanced Technology Materials Co., Ltd., Beijing 100086, China;

    Engineering and Technology Research Center of Hot Isostatic Pressing, Zhuozhou Hebei 072750, China;

    Advanced Technology Materials Co., Ltd., Beijing 100086, China;

    Engineering and Technology Research Center of Hot Isostatic Pressing, Zhuozhou Hebei 072750, China;

    Advanced Technology Materials Co., Ltd., Beijing 100086, China;

    Engineering and Technology Research Center of Refractory Materials, Beijing 100083, China;

  • 会议组织
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类 金属学与热处理;
  • 关键词

    pitting corrosion; HIP; ST12; AES;

    机译:点蚀; HIP; ST12; AES;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号