首页> 外国专利> Wool-like polyester filament and its manufacturing method

Wool-like polyester filament and its manufacturing method

机译:仿毛涤纶长丝及其制造方法

摘要

An object of the present invention is to provide a wool-like polyester filament and a method for producing the same. The method for producing wool-like polyester filaments is terephthalic acid, 1,4-butanediol, fluorine-containing dicarboxylic acid, hexanediol having tert-butyl, and 2,5,6,6-tetramethyl-2,5-heptanediol. Is uniformly mixed and further esterified, and the melt of the modified polyester to be polycondensed is made into a fiber by a method of semi-drawn yarn (Partially Oriented Yarn, POY) and drawn processed yarn (Draw Textured Yarn, DTY). That is. The obtained fibers had a dyeing rate of 90.32 to 93.27% at a dyeing temperature of 100 ° C., a dyeing performance of K / S value of 22.15 to 23.42, and a relative humidity of 25 ° C. and 65%. After being placed underneath for 60 months, it has a natural decomposition performance of 18 to 25% of the intrinsic viscosity decrease. The method provided in the present invention has a wide range of uses because the cost is low, the operation is convenient, and the provided product has good dyeing performance and fast natural biodegradation. [Selection diagram] Fig. 1
机译:本发明的目的是提供一种仿毛聚酯长丝及其生产方法。生产羊毛状聚酯长丝的方法是对苯二甲酸、1,4-丁二醇、含氟二羧酸、具有叔丁基的己二醇和2,5,6,6-四甲基-2,5-庚二醇。通过半拉伸纱线(部分取向纱线,POY)和拉伸加工纱线(拉伸变形纱线,DTY)的方法将待缩聚的改性聚酯熔体制成纤维。就是这样。在100°C的染色温度下,所得纤维的染色率为90.32%至93.27%,K/S值为22.15至23.42,相对湿度为25°C和65%。放置60个月后,其自然分解性能为特性粘度降低的18%至25%。本发明方法成本低,操作方便,产品染色性能好,自然降解快,用途广泛。[选择图]图1

著录项

  • 公开/公告号JP7053956B2

    专利类型

  • 公开/公告日2022-04-12

    原文格式PDF

  • 申请/专利权人 江蘇恒力化繊股▲ふん▼有限公司;

    申请/专利号JP20210524973

  • 发明设计人 王 山水;王 麗麗;沈 建根;

    申请日2019-10-28

  • 分类号D01F6/84;C08G63/682;C08G63/78;C08G63/85;D02J1/22;C25B3/25;C25B3/07;C07C31/20;C07C29/17;C07B61;

  • 国家 JP

  • 入库时间 2022-08-25 00:30:31