The present invention relates to a cement admixture composition applied to an on-site hydration concrete mat, which is cured while exhibiting rapid expansibility in the initial stage, a fast-expansion hardening type cement admixture composition preferably using the same, an in-situ hydration concrete mat, and a preferred construction method of the concrete mat . The rapid water expansion hardening type cement mixture composition according to the present invention comprises: 25 to 65 wt% of crude cement having a specific surface area of 4,000-5,200 cm 2 /g; 5.0 to 20% by weight of calcined magnesium oxide powder having a specific surface area of 5,000 to 6,000 cm 2 /g; 0.1-0.6 wt% of a high-viscosity thickener having a viscosity of 45,000-65,000 cpa; 5.5-15 wt% of CSA-based clinker powder; Anhydrite 3.0-10 wt%; Dry silica sand 20-25 wt%; 0.2 to 2.0 wt% of a setting retarder; 0.3 to 1.6 wt% of a superplasticizer; Anti-foaming agent 0.2 to 0.8% by weight; characterized in that it comprises a composition. This rapid water expansion hardening type cement mixture composition can be filled in the space surrounded by the fiber cover and made into a roll-type on-site hydration concrete mat.
机译:本发明涉及应用于现场水化混凝土垫的水泥混合物组合物,其在初始阶段在表现出快速扩展的同时固化,优选使用相同的快速膨胀硬化型水泥混合物组合物,其原位水合混凝土垫,以及混凝土垫的优选施工方法。根据本发明的快速水膨胀硬化型水泥混合物组合物包含:25至65重量%的粗水泥,具有4,000-5,200cm 2 / g的比表面积; 5.0至20重量%的煅烧氧化镁粉末,特定表面积为5,000至6,000cm 2 / g; 0.1-0.6重量%的高粘度增稠剂,粘度为45,000-65,000cpa; 5.5-15%的基于CSA的熟料粉末; Anhydite 3.0-10wt%;干硅砂20-25wt%; 0.2至2.0wt%的设置延迟器; 0.3至1.6wt%的超塑化剂;抗发泡剂0.2至0.8重量%;其特征在于它包括组合物。这种快速的水膨胀型硬化型水泥混合物组合物可以填充在由纤维盖包围的空间中,并制成辊式现场水化混凝土垫。

著录项

  • 公开/公告号KR102349613B1

    专利类型

  • 公开/公告日2022-01-13

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR1020210103676

  • 发明设计人 박동철;박재범;이정우;이영화;

    申请日2021-08-06

  • 分类号C04B28/16;C04B14/06;C04B14/10;C04B14/30;C04B20/02;C04B20/04;C04B22;C04B24/42;C04B40/02;C04B7;C04B7/32;

  • 国家 KR

  • 入库时间 2022-08-24 23:27:24

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号