首页> 外国专利> FIBROUS MATERIAL IMPREGNATED WITH THERMOPLASTIC POLYMER OF THICKNESS LESS THAN OR EQUAL TO 100ΜM AND ITS PREPARATION PROCESS

FIBROUS MATERIAL IMPREGNATED WITH THERMOPLASTIC POLYMER OF THICKNESS LESS THAN OR EQUAL TO 100ΜM AND ITS PREPARATION PROCESS

机译:纤维材料浸渍有厚度小于或等于100μm的热塑性聚合物及其制备方法

摘要

The present invention relates to an impregnated fibrous material comprising at least one continuous fiber fibrous material and: - at least one non-reactive thermoplastic polymer matrix, or - at least one reactive thermoplastic prepolymer, precursor of said non-reactive thermoplastic polymer, optionally mixed with a chain extender, characterized in that said at least non-reactive thermoplastic polymer or said reactive prepolymer is an amorphous polymer or prepolymer whose glass transition temperature is such that Tg ≥ 80 ° C, in particular Tg ≥ 100 ° C, in particular ≥ 120 ° C, in particular ≥ 140 ° C, or is a semi-crystalline polymer or prepolymer with a melting point Tf ≥ 150 ° C, the fiber content in said prepreg fibrous material being from 45 to 65% in volume, preferably from 50 to 60% by volume, in particular from 54 to 60%, the average thickness of said impregnated fibrous material being less than or equal to 100 μm, independently of the number of fibers present ntes in said fibrous material before impregnation.
机译:本发明涉及浸渍的纤维材料,其包含至少一种连续纤维纤维材料和: - 至少一种非反应性热塑性聚合物基质,或 - 至少一种反应性热塑性预聚物,所述非反应性热塑性聚合物的前体,任选地混合用链子增量剂,其特征在于,所述至少非反应性热塑性聚合物或所述反应性预聚物是非晶聚合物或预聚物,其玻璃化转变温度使得Tg≥80℃,特别是Tg≥100℃,特别是≥ 120°C,特别是≥140℃,或者是半结晶聚合物或预聚物,具有熔点TF≥150℃,所述预浸料纤维材料中的纤维含量为45%至65%,优选为50对于60%(体积),特别是54〜60%,所述浸渍纤维材料的平均厚度小于或等于100μm,独立于所述纤维中的纤维数目XTES浸渍前的美国材料。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号