首页> 外国专利> CU-CR-ZR ALLOY CONTACT LINE FOR ELECTRIFIED RAILWAYS AND MANUFACTURING METHOD THEREFOR

CU-CR-ZR ALLOY CONTACT LINE FOR ELECTRIFIED RAILWAYS AND MANUFACTURING METHOD THEREFOR

机译:电气化铁路CU-CR-ZR合金接触线及其制造方法

摘要

A Cu-Cr-Zr alloy, a manufacturing method therefor, a Cu-Cr-Zr alloy contact line for electrified railways and a manufacturing method therefor. The chemical composition and weight percentage of the Cu-Cr-Zr alloy are as follows: Cr: 0.2%-1.0%, Zr: 0.02-0.2%, and the balance being Cu. The manufacturing method for the Cu-Cr-Zr alloy material contact wire for high-speed railways comprises the following steps: (1) in an inert atmosphere, subjecting an alloy solution to an upper casting process to obtain a copper rod blank; and (2) subjecting the copper rod blank in step (1) to hot rolling treatment, solid solution treatment, cold rolling treatment and aging treatment. Said method realizes large-length and large-unit-weight industrial production of a Cu-Cr-Zr contact wire for high-speed railways, has the advantages of excellent performance, stable quality, continuous operation and high material utilization rate, and can realize large-scale production.
机译:一种Cu-Cr-Zr合金,其制造方法,用于电气化铁路的Cu-Cr-Zr合金接触线及其制造方法。 Cu-Cr-Zr合金的化学成分和重量百分比如下:Cr:0.2%-1.0%,Zr:0.02-0.2%,余量为Cu。 用于高速铁路的Cu-Cr-Zr合金材料接触线的制造方法包括以下步骤:(1)在惰性气氛中,使合金溶液进行上浇铸过程以获得铜棒坯料; (2)在步骤(1)中经受铜杆坯料至热轧处理,固溶处理,冷轧处理和老化处理。 所述方法实现了高速铁路Cu-Cr-Zr接触线的大长和大单位的工业生产,具有优异的性能,质量稳定,持续运行,材料利用率高,并可实现 大规模生产。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号