Pure phase for Fischer Tropsch synthesis ε/ε’ Iron carbide catalyst, method for producing same, and Fischer Tropsch synthesis method

机译:纯相对于幼零滴合成ε/ε'1铁碳化物催化剂,其制备方法和费城鼠合成方法

摘要

The present invention relates toPure phase for Fischer Tropsch synthesis ε/ε’ Iron carbide catalystManufacturing method and Fischer Tropsch synthesis methodManufacturing method isNano powder iron compounds capable of obtaining nanoiron powders by nanoiron powder or in situ reductionThe process of cleaning the surface at temperatures of 250 to 510(2) the material obtained in stepH2, the molar ratio of H2 to CO is 1.2 toPretreatment with CO at a temperature of 80 to 180(3) the material obtained in stepH2, the molar ratio of H2 to CO is from 1.0 to 3.0Manufacturing a carbide at a temperature of 180 to 280.This manufacturing method is easy to obtain raw material, convenient operation process, and 100% pure phase ε/ε’ The iron carbide catalyst can be produced, and this catalyst is low in CO2 and CH4 selectivity, and the selectivity of the effective product is high.
机译:本发明涉及Fischer Tropsch合成ε/ε'1'铁碳化物催化剂制造方法和Fischer Tropsch合成方法制造方法制备方法制备方法制备方法纳米铁粉末或原位减少在250至250的温度下清洁表面的过程制备方法制备方法。 510(2)在梯楦中获得的材料,H 2 TO CO的摩尔比为1.2在80-180(3)所述的CO的摩尔比,在Steph2中获得的材料,H 2 TO CO的摩尔比为1.0至3.0 在180至280的温度下制造碳化物。该制造方法易于获得原料,方便的操作方法,和100%纯相ε/ε'可以制备铁碳化铁催化剂,并且该催化剂在二氧化碳中低低 CH4选择性,有效产品的选择性高。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号