FIELD: metallurgy. ;SUBSTANCE: invention relates to the field of metallurgy, namely to the casting of high-strength wear-resistant steel used for the manufacture of the main working bodies and structural elements of mining transport and mining equipment. Steel contains, by wt. %: carbon 0.25-0.35, silicon 0.20-0.45, manganese 0.80-1.20, chromium 1.00-1.50, molybdenum 0.20-0.40, nickel 1.0-1.50, copper no more than 0.30, niobium 0.008-0.10, vanadium 0.08-0.10, calcium 0.005-0.01, barium 0.005-0.01, cerium 0.005-0.01, zirconium 0.008-0.1, aluminum 0.008-0.05, sulfur is no more than 0.015, phosphorus no more than 0.015, nitrogen is not more than 0.025, zirconium carbonitride nanoparticles and niobium carbonitride nanoparticles are 0.04-0.25, the rest is iron and impurities. ;EFFECT: invention provides increased strength, wear resistance, impact strength and ductility of the casting steel. ;6 cl, 2 tbl
机译:领域:冶金。 ;物质:发明涉及冶金领域,即铸造高强度耐磨钢,用于制造主要工作体和采矿设备的结构元素。 钢含有wt。 % : 碳 0.25-0.35 , 硅 0.20-0.45 ,锰 0.80〜1.20 ,铬 1.00-1.50 ,钼 0.20-0.40 ,镍 1.0-1.50 ,铜 不超过 0.30 ,铌 0.008-0.10 ,钒 0.08-0.10 ,钙 0.005 -0.01,钡0.005-0.01,铈0.005-0.01,氧化锆0.008-0.05,硫比不大于0.015,磷不大于0.015,氮素不大于0.025,碳氮化酰胺纳米粒子和铌碳氮化碳纳米铵纳米粒子 为0.04-0.25,其余的是钢铁和杂质。 ;效果:发明提供了铸钢的强度,耐磨性,冲击强度和延展性。 ; 6 cl,2 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号