METHOD FOR RESTORATION OF WORKING MEMBERS OF TILLING MACHINERY

机译:恢复耕地机械工作成员的方法

摘要

FIELD: metal working.;SUBSTANCE: invention relates to restoration of worn parts using welding and can be used the restoration of working bodies of tilling machines. In the method, ball-bearing strip steel ShKh9, 12 mm wide, 5 mm thick, is used, the strips are cut to the size of the cutting part and welded parallel to the cutting part, hardening is executed by electric arc submerged surfacing with direct current of reverse polarity at a current strength of 160 to 225 A, diameter of the electrode wire 1.8 to 2.2 mm, voltage 30 to 33 V, surfacing rate 20 to 25 m/h and electrode wire supply rate 110 to 120 m/h, and electrode wire is used as a wear-resistant material with the following contents, % wt.: С - 1.8, Mn - 0.9, Si - 2.2, Al - 1.1, Cr - 9.2, Ni - 8.2, V - 0.6, Mo - 1.0, Fe the rest, wherein the thickness of the deposited layer is 1.8 to 2.2 mm, and the hardness thereof is 61 to 62 HRC.;EFFECT: invention allows improving hardness and wear resistance of the restored working members under conditions of intense abrasive wear.;1 cl, 2 ex
机译:领域:金属工作。物质:发明涉及使用焊接的磨损部件的恢复,并可以使用耕作机械的工作体的恢复。在该方法中,使用滚珠带钢SHKH9,12mm宽,5mm厚,将条带切割成切割部分的尺寸并平行焊接到切割部分,通过电弧浸没表面执行硬化。反极性的直流电流在电流强度为160至225a,电极线的直径1.8至2.2 mm,电压30至33 V,浮出率20至25m / h,电极线供应速率110至120 m / h和电极线用作具有以下内容物的耐磨材料,%wt .:с - 1.8,Mn-0.9,Si-2.2,Al - 1.1,Cr-9.2,Ni-8.2,V - 0.6,Mo - 1.0,Fe The,其中沉积层的厚度为1.8至2.2mm,并且其硬度为61至62hrc。;效果:发明允许在强烈磨料的条件下提高恢复的工作构件的硬度和耐磨性磨损。; 1 cl,2前

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号