The present invention discloses low steel grade pipeline clean steel, and relates to the field of metallurgical technology, the chemical composition and mass percentage of which are C: 0.04% to 0.07%, Si: 0.10% to 0.35%, Mn: 1.00% to 1.50%, P≤0.015%, S:0.0020%~0.0050%, Nb:0.030%~0.070%, Ti:0.006%~0.020%, Ni≤0.30%, Cr≤0.30%, Cu≤0.30%, Al:0.015 %~0.050%, the remainder is Fe and impurities. The present invention systematically and accurately analyzes the formation control mechanism of inclusions, carries out the calcium treatment method after RH vacuum treatment through rational component design, and achieves the purpose of improving the purity of molten iron by rationally controlling the degree of superheat, thereby achieving the internal quality of steel and improve the economic effect.
机译:本发明公开了低钢级管道清洁钢,涉及冶金技术领域,化学成分和质量百分比为C:0.04%至0.07%,Si:0.10%至0.35%,Mn:1.00%至 1.50%,P≤0.015%,S:0.0020%〜0.0050%,Nb:0.030%〜0.070%,Ti:0.006%〜0.020%,Ni≤0.30%,Cr≤0.30%,Cu≤0.30%,Al:0.015 %〜0.050%,其余的是Fe和杂质。 本发明通过理性分量设计系统地和精确地分析了夹杂物的形成控制机制,通过合理组分设计进行了RH真空处理后的钙处理方法,通过合理控制过热程度来实现改善铁水纯度的目的,从而实现 内部质量的钢材,提高经济效益。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号