摘要

The present invention relates to a method for manufacturing a composite street lamp using domestic oak, which allows the use of high value-added products for domestic oak, particularly oak thinning, to be significantly increased while preventing splitting and twisting of oak during drying so that the product is stably manufactured. The present manufacturing method relates to a raw wood cut lumber preparation step (S10) of preparing raw wood cut lumber by sawing oak, and a heating plate installation step (S20) of laminating the raw wood block lumber and a heating plate on a bogie to form a laminated wood (S20), and the bogie A drying chamber sealing step (S30) of putting into the drying chamber and sealing the drying chamber, a vacuum forming step (S40) of forming a vacuum inside the drying chamber, and the pressure plate by forming the vacuum A vacuum pressurizing step (S50) of pressurizing the laminated wood, a raw wood drying step (S60) of circulating hot water through the heating plate to dry the raw wood block material to form a dried wood block material, and the interior of the drying chamber during the drying of the green wood block material A pressing pressure adjusting step (S70) of adjusting the pressing force by the pressing plate, a room temperature cooling step (S80) of cooling the dried rectangular wood, and a high heat treatment step of treating the dried rectangular wood with high heat (S90), and two It includes a wooden lamp pole forming step (S100) of processing and bonding the dried square material to form a wooden lamp post, and an outer surface processing step (S110) of processing the outer surface of the wooden lamp pole into a cylindrical shape to complete the street lamp pole.
机译:本发明涉及一种使用国内橡木制造复合路灯的方法,这允许使用高附加值的产品用于国内橡木,特别是橡木稀薄,在干燥期间防止橡木的分裂和扭曲橡木的分裂和扭曲该产品是稳定制造的。本发明的制造方法涉及通过锯切橡木制备原木切割木材的原木切割木材制备步骤(S10),以及将原木块木材和加热板上的加热板安装步骤(S20)上的加热板安装步骤(S20)上形成层压木材(S20),并将转向架是放入干燥室中并密封干燥室的干燥室密封步骤(S30),真空形成步骤(S40)在干燥室内形成真空,以及压力通过形成真空加压步骤(S50)的真空加压步骤(S50),通过加热板循环热水的原木干燥步骤(S60),以使原木块材料干燥,形成干燥的木块材料,干燥室的内部在绿色木块的干燥过程中,压力调节步骤(S70)通过压板调节压力,冷却干燥的矩形W的室温冷却步骤(S80) ood和高热处理步骤用高热量处理干燥的矩形木材(S90)和两个,它包括一个木灯杆形成步骤(S100)的加工和粘合干燥的方形材料,形成木灯柱,将木灯杆的外表面处理成圆柱形状的外表面处理步骤(S110)以完成路灯杆。

著录项

  • 公开/公告号KR102270608B1

    专利类型

  • 公开/公告日2021-06-30

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR1020190133200

  • 发明设计人 문중묵;

    申请日2019-10-24

  • 分类号B27M3/32;B27H5/04;B27H5/08;B27K5;B27M1/08;B27M3;E04H12/04;F21S8/08;F21W131/103;

  • 国家 KR

  • 入库时间 2022-08-24 19:51:56