Electrical steel sheet and its manufacturing method, rotor motor core and its manufacturing method, stator motor core and its manufacturing method, and motor core manufacturing method

机译:电钢板及其制造方法,转子电机芯及其制造方法,定子电机芯及其制造方法,以及电机芯制造方法

摘要

To provide an electromagnetic steel that suppresses decrease in magnetic flux density during annealing for removing distortions and a method of producing the same.SOLUTION: An electromagnetic steel contains Si of 2.0 mass% or more and 4.5 mass% or less and Mn of 2.5 mass% or more and 5.0% mass or less, and further contains at least one element selected from Ca, Mg, Ce, Ti, Ba, and Be in a total of 0.0001 mass% or more and 0.1 mass% or less, with Al of less than 0.03 mass%, C of less than 0.002 mass%, and S of less than 0.002 mass%, the steel having Fe as the main component. The steel has an average crystal grain size of 60 μm or more and 80 μm or less.SELECTED DRAWING: Figure 1
机译:提供一种电磁钢,其在退火期间抑制磁通密度的降低,以消除扭曲和制造方法。溶液:电磁钢含有2.0质量%以上的Si,4.5质量%或更低,Mn为2.5质量%。或者更多和5.0%或更低,还含有至少一种选自Ca,Mg,Ce,Ti,Ba的元素,并且总共0.0001质量%或更高,并具有较低的al超过0.002质量%的0.03质量%,并且S小于0.002质量%,钢具有Fe作为主要成分。钢的平均晶粒尺寸为60μm以上且80微米或更小。选择图:图1

著录项

  • 公开/公告号JP6891682B2

    专利类型

  • 公开/公告日2021-06-18

    原文格式PDF

  • 申请/专利权人 日本製鉄株式会社;

    申请/专利号JP20170137275

  • 发明设计人 冨田 美穂;藤村 浩志;

    申请日2017-07-13

  • 分类号C22C38;C22C38/14;C21D8/12;H01F1/147;C22C38/60;

  • 国家 JP

  • 入库时间 2022-08-24 19:33:34