A Ti-containing ferritic stainless steel sheet for an exhaust pipe flange member has a composition containing, in mass percentage, from 0.003 to 0.030% of C, 2.0% or less of S i, 2.0% or less of Mn, 0.050% or less of P, 0.040% or less of S, from 10.0 to 19.0% of Cr, 0.030% or less of N, from 0.07 to 0.50% of Ti, from 0.010 to 0.20% of Al, from 0 to 1.50% of Mo, and from 0 to 0.0030% of B, with the balance Fe and unavoidable impurities, has a K value of 150 or more, has a sheet surface hardness of 170 HV or less, and has a sheet thickness of from 5.0 to 11.0 mm. The K value equals −0.07×Cr−6790×Free(C+N)−1.44×d+267, wherein Free(C+N) corresponds to the solid-dissolved (C+N) concentration (% by mass), and d represents an average crystal grain diameter (μm).
机译:用于排气管凸缘构件的含Ti的铁素体不锈钢片的含有含有质量百分比的组合物,0.003至0.030%的C,2.0%或更低的S I,2.0%或更少的Mn,0.050%或更低P,0.040%或更少的S,0.0%至19.0%的CR,0.030%或更低的N,0.07至0.50%的Ti,从0.010-0.20%,从00-1.50%的Mo,和B的0至0.0030%,具有余量的Fe和不可避免的杂质,具有150或更大的k值,具有170 HV或更低的片状硬度,并且具有5.0至11.0mm的薄片厚度。 K值等于-0.07×Cr-6790×自由(C + N)-1.44×D + 267,其中游离(C + N)对应于固溶体(C + N)浓度(质量%),和D表示平均晶粒直径(μm)。

著录项

  • 公开/公告号US10995888B2

    专利类型

  • 公开/公告日2021-05-04

    原文格式PDF

  • 申请/专利权人 NISSHIN STEEL CO. LTD.;

    申请/专利号US201716098150

  • 申请日2017-02-07

  • 分类号C21D8/02;C22C38/02;F16L23/032;C21D6;C21D8;C21D9/46;C22C38;C22C38/04;C22C38/06;C22C38/22;C22C38/28;C22C38/32;F01N13/16;F01N13/18;

  • 国家 US

  • 入库时间 2022-08-24 18:32:02

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号