The present invention in the fast-setting cement concrete composition with improved long-term durability, fast-setting mixed material 5 to 45% by weight, fine aggregate 30 to 60% by weight, coarse aggregate 15 to 60% by weight, latex modifier 3 to 20% by weight, and water 2 Containing to 25% by weight, the fast-setting mixture is crude steel Portland cement 20 to 80 parts by weight, magnesium sulfoaluminate 10 to 50 parts by weight, amorphous tricalcium aluminate 1 to 30 parts by weight, mullite 5 to 20 parts by weight , 0.01 to 10 parts by weight of alkylene amide, 0.01 to 10 parts by weight of propylene glycol alginate, 0.01 to 10 parts by weight of calcium stearate, and 0.5 to 10 parts by weight of calcium aluminate, and the latex modifier is 30 to 65 parts by weight of chloroprene rubber , 10 to 30 parts by weight of siloxane rubber of a network structure, 15 to 30 parts by weight of cellulose nanofibers having a lignin content of 25 to 40% by weight and a hydroxymethyl group not modified with a carboxylic acid or salt thereof, and 1 to 30 parts by weight of a natural shellac resin Containing 10 parts by weight, and maintaining watertightness, adhesion, durability, and crack resistance, and excellent chloride penetration resistance and freeze-thaw resistance according to temperature change, the fast-setting cement concrete composition and road pavement maintenance method with improved long-term durability. will be.
机译:本发明在快速设定的水泥混凝土组合物中具有改善的长期耐久性,快速设定混合材料5至45重量%,细聚集体30至60重量%,粗骨料15至60重量%,胶乳改性剂3至20重量%,水2含有25重量%的水,快速设定的混合物是粗钢板料水泥水泥20至80重量份,硫化镁10至50重量份,无定形三钙铝酸盐1至30重量份按重量,莫来石莫来5至20重量份,0.01至10重量份的亚烷基酰胺,0.01至10重量份丙二醇藻酸盐,0.01至10重量份的硬脂酸钙,0.5至10重量份铝酸钙,乳胶改性剂为30至65重量份的氯丁烯橡胶,10至30重量份的网络结构的硅氧烷橡胶,15至30重量份的纤维素纳米纤维,具有25%至40%的木质素含量重量和羟甲基不是m用羧酸或其盐,1至30重量份含有10重量份的天然虫胶树脂,并保持水密性,粘合,耐久性和抗裂性,以及优异的氯化物穿透性和冻土抗性温度变化,快速设定水泥混凝土组成和道路路面维护方法,具有改善的长期耐久性。将。

著录项

  • 公开/公告号KR102229897B1

    专利类型

  • 公开/公告日2021-03-22

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR1020200119608

  • 发明设计人 유세균;

    申请日2020-09-17

  • 分类号C04B28/06;C04B20;C04B22;C04B24/08;C04B24/12;C04B24/26;C04B24/38;C04B41/45;C04B7/02;C08L11;C08L83/04;

  • 国家 KR

  • 入库时间 2022-08-24 17:50:06

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号