FIELD: chemistry.;SUBSTANCE: invention relates to method for producing a catalyst for hydrotreating diesel fractions containing Co, Mo and P, including preparation of a solution of complex salts [P2Mo5O23]6-, [РМо12О40]3-, [РМо11О40]3-, [P2Mo18O42]6-, [PMo9O31(ОН)3]6- heteropolyanions, or mixtures thereof, using H3PO4 and an organic modifier, the combination and ratios of which provide the formation of heteropolyacid anions in solution [P2Mo5O23]6-, [РМо12О40]3-, [РМо11О40]3-, [P2Mo18O42]6-, [PMo9O31(ОН)3]6-, or their mixtures and their stability at pH in the range from 0.7 to 4.5, evacuation and impregnation of the support with a solution of complex salts [P2Mo5O23]6-, [РМо12О40]3-, [РМо11О40]3-, [P2Mo18O42]6-, [PMo9O31(ОН)3]6- heteropolyanions, or mixtures thereof, maturation of the impregnated catalyst and drying to obtain samples, the content of components in which corresponds to the content of oxides CoO, MoO3 and P2O5 in the sample calcined for 2 hours at 550°C, equal to 2.2-6.2 wt.%, 14.0-30.0 wt.% and 0.6-4.9 wt.% respectively, heat-resistant alumina support - the rest, and further activation of the samples in a stream of hydrogen when feeding a mixture of dimethyl disulfide-oil fraction. The invention also relates to a catalyst for hydrotreating diesel fractions obtained by the above-described method and to a method for hydrotreating a diesel fraction using the claimed catalyst.;EFFECT: highly active hydrotreating catalyst that allows the production of diesel fuel components that meet the quality of modern regulatory requirements.;18 cl, 7 tbl, 24 ex
机译:领域:化学。物质:发明内容涉及用于制备含有CO,Mo和P的柴油级分的催化剂的方法,包括制备复合物盐的溶液[P 2 Mo 5 < / sub> O 23 ] 6 - ,[рмо 12 о 40 ] 3 - ,[рмо 11 40 ] 3 - ,[p 2 mo 18 O 42 ] 6 - ,[pmo 9 O 31 (он) 3 2 mo] 5 O 23 ] 6 - ,[рмо 12 о 40 ] 3 - ,[рмо 11 40 ] 3 - ,[p 2 mo < Sub> 18 O 42 ] 6 - ,[pmo 9 O 31 (он)<亚> 3 ] 6 - ,或它们的混合物,它们在pH下的稳定性为0.7至4.5,疏散和用复合盐的溶液浸渍载体[P 2 Mo 5 O 23 ] 6 - ,[ рмо 12 40 ] 3 - ,[рмо 11 40 ] < sup> 3 - ,[p 2 mo 18 O 42 ] 6 - ,[pmo <亚> 9 O 31 (он) 3 ] 6 - 杂阳极,或其混合物,浸渍催化剂的成熟和取得样品的干燥,其组分的含量对应于在550℃下煅烧2小时的样品中氧化物CoO,MOO3和P2O5的含量,等于2.2-6.2重量%,14.0-30.0重量%和0.6-4.9重量%分别,耐热氧化铝载体 - 其余的,以及在氢气中喂养二甲基二硫化物馏分的混合物时,进一步激活氢气流中的样品。本发明还涉及通过上述方法获得的加氢处理柴油级分的催化剂,以及使用所要求保护的催化剂加氢处理柴油级分的方法。;效果:高活性加氢处理催化剂,允许生产柴油燃料组件现代监管要求的质量。; 18 cl,7 tbl,24前

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号