PROBLEM TO BE SOLVED: To provide a wrap film having an excellent feel to the touch and suppressing tear trouble and deterioration of pullability. SOLUTION: The low temperature crystallization start temperature measured by a temperature-modulated differential scanning calorimeter containing a vinylidene chloride resin and an epoxidized fatty acid alkyl ester having a viscosity at 30 ° C. of 100 mPa · s or less is determined. A wrap film having a temperature of 40 to 60 ° C. and a thickness of 6 to 18 μm. [Selection diagram] None