The mechanical properties of alloys consisting of copper and 0,2-3,0 per cent of chromium are improved by heating the alloys at temperatures between 700 DEG C. and the melting-point of the alloys, quenching and ageing at 350-700 DEG C. or working the alloys at above 700 DEG C., cooling in the air and then heating to 350-700 DEG C. The alloys may also contain 1-10 per cent of aluminium, and additions of one or more elements other than beryllium, titanium, or silicon which do not combine with chromium such as 1-10 per cent of nickel, 1-10 of tin, and 1-20 of zinc. The improved alloys may be used for the manufacture of fire boxes or parts thereof.
机译:通过在700℃至合金熔点之间加热,在350-700℃淬火和时效来改善由铜和0.3%至0.2%铬组成的合金的机械性能。或在高于700℃的温度下加工合金,然后在空气中冷却,然后加热至350-700℃。合金还可以包含1-10%的铝,并添加一种或多种铍以外的元素,钛或不会与铬结合的硅,例如镍的1-10%,锡的1-10和锌的1-20。改进的合金可用于制造火箱或其零件。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号